FIELD: ores and rocks grinding. SUBSTANCE: ore is treated with bacterial culture Thiobacillus ferrooxidans at concentration 0.04-0.12 kg biomass/t ore at the ratio solid:liquid = (4-5):1, at 15-35 C, at pH 1.5-2.3 for 3-12 days. EFFECT: improved method of ore grinding. 3 tbl
Title | Year | Author | Number |
---|---|---|---|
INTEGRATED WASTELESS METHOD FOR PROCESSING MANGANESE ORES | 1996 |
|
RU2095453C1 |
COMBINED METHOD OF REBELLIOUS LEAD-ZINC ORES PROCESSING | 2015 |
|
RU2601526C1 |
METHOD OF MANGANESE HEAP BIOLEACHING OF MANGANESE-CONTAINING MATERIALS | 2018 |
|
RU2686158C1 |
METHOD OF THE URANIUM LEACHING FROM THE ROCKS WITH ITS INSIGNIFICANT CONTENT | 2016 |
|
RU2653400C2 |
METHOD FOR EXTRACTION OF GOLD FROM RESISTANT FINE GROUND SULPHIDE CONCENTRATES | 2021 |
|
RU2798854C2 |
METHOD OF CONCENTRATION OF POOR AND BALANCED SILVER-CONTAINING SULPHIDE ORES AND CONCENTRATION TAILINGS | 2014 |
|
RU2555280C1 |
METHOD FOR EXTRACTING COPPER FROM SULPHIDE-BEARING ORE | 2011 |
|
RU2471006C1 |
METHOD OF FLOTATION CONCENTRATION OF CAKE OF SULPHURIC ACID LEACHING OF COPPER ORE | 2007 |
|
RU2350396C2 |
METHOD OF PROCESSING SULFIDE GOLD-BEARING CONCENTRATES | 2005 |
|
RU2283358C1 |
HEAP BIOLOGICAL LEACHING LEAN REFRACTORY MINERAL RAW MATERIALS OF NATURAL AND TECHNOGENIC ORIGIN | 2017 |
|
RU2679724C1 |
Authors
Dates
1996-03-27—Published
1994-02-03—Filed