FIELD: automobile engineering. SUBSTANCE: desired composition contains (mass parts): epoxy diane resin 50-95, furfural 10-40, solution of diethylene triaminomethyl phenol in acetone (their ratio being 2:1) 30-95, polybenzyl pyridinium chloride (its molecular weight being 420) 0.02-2.8, perchlorvinyl resin 0.03-3.0, basalt scales 5-250. EFFECT: improves quality of desired coating. 2 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| POLYMER COMPOSITION FOR PROTECTIVE BARRIER-TYPE ANTICORROSION COATING | 2008 |
|
RU2394058C2 |
| POLYMER COMPOUND FOR PROTECTIVE CORROSION-RESISTANT BARRIER-TYPE COATING | 2007 |
|
RU2351624C1 |
| POLYMERIC PROTECTIVE BARRIER COATING | 2006 |
|
RU2306325C1 |
| WEAR-RESISTANT POLYMERIC COMPOSITION | 1991 |
|
SU1825514A3 |
| HEAT-RESISTANT ANTIFOULING POLYMER COMPOSITION FOR COATINGS | 1992 |
|
RU2028347C1 |
| ACIDPROOF POLYMER COMPOSITION FOR COATINGS | 1991 |
|
SU1825510A3 |
| WATER RESISTANCE AND CRACK-RESISTING POLYMER COMPOSITION | 1992 |
|
SU1831870A3 |
| CHEMICALLY RESISTANT POLYMER COMPOSITION FOR COATINGS | 1992 |
|
SU1831871A3 |
| METHOD OF MINERAL FIBROUS MATERIAL TREATMENT | 1990 |
|
RU2023692C1 |
| METHOD OF HEAT TREATMENT OF DISPERSED FLAKE-LIKE PARTICLES AND DEVICE FOR ITS FULFILLMENT | 1991 |
|
RU2036748C1 |
Authors
Dates
1996-03-27—Published
1992-05-26—Filed