FIELD: production of fiber glass and basalt plastic materials. SUBSTANCE: mineral fibrous materials are treated with a aqueous solution containing 5-15 wt. -% amine hardener and 4-9 wt.-% benzylpyridinium chloride for 30-240 s. Rate is 0.5-0.8 l/min at the linear fiber stretching rate 2950 m/min. Adhesion to the epoxy-binder is 5-22 MPa. EFFECT: improved method of mineral fibrous material treatment. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
LUBRICANT FOR CONTINUOUS BASALT FIBER | 2021 |
|
RU2790641C2 |
0 |
|
SU1781182A1 | |
COMPOSITION FOR TREATING MINERAL FIBER | 0 |
|
SU1775377A1 |
MODIFIED POLYMER COMPOSITE REINFORCEMENT | 2023 |
|
RU2826026C1 |
OIL- AND BENZO-RESISTANT POLYMER COMPOSITION FOR COATINGS | 1992 |
|
RU2057157C1 |
CHEMICALLY RESISTANT POLYMER COMPOSITION FOR COATINGS | 1992 |
|
SU1831871A3 |
HEAT-RESISTANT ANTIFOULING POLYMER COMPOSITION FOR COATINGS | 1992 |
|
RU2028347C1 |
POLYMERIZABLE COMPOSITE MATERIAL | 1996 |
|
RU2119515C1 |
ACIDPROOF POLYMER COMPOSITION FOR COATINGS | 1991 |
|
SU1825510A3 |
WATER RESISTANCE AND CRACK-RESISTING POLYMER COMPOSITION | 1992 |
|
SU1831870A3 |
Authors
Dates
1994-11-30—Published
1990-07-30—Filed