FIELD: production of mineral tanning agent. SUBSTANCE: method involves preparing solution of titanyl sulfate, its mixing and cooling followed by salting out sulfatotitanyl of ammonium. Mixture of product being prepared by evaporation of mother solution which is obtained after filtration of suspension of titanium tanning agent and ammonium sulfate at their ratio not more 3:1 is used as mentioned above salting agent. EFFECT: improves efficiency of method. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCTION OF TITANIUM TANNING AGENT FOR LEATHER | 1994 |
|
RU2057184C1 |
METHOD FOR PRODUCTION OF TITANIUM TANNING AGENT FOR LEATHER | 1994 |
|
RU2078140C1 |
METHOD OF PREPARING TITANIUM TANNING AGENTS FOR SKIN | 1996 |
|
RU2103372C1 |
METHOD OF PREPARING TITANIUM TANNING AGENT FOR LEATHER | 1995 |
|
RU2113492C1 |
FILTER MEDIUM | 1995 |
|
RU2104748C1 |
TITANIUM TANNING AGENT | 1995 |
|
RU2112809C1 |
METHOD OF PRODUCING MINERAL TANNING AGENT | 2012 |
|
RU2509810C1 |
METHOD OF PROCESSING SPHENE CONCENTRATE | 2009 |
|
RU2394768C1 |
METHOD OF PRODUCING TITANIUM TANNING AGENT | 2012 |
|
RU2484143C1 |
METHOD OF PREPARING TITANIUM HARDENER FROM TITANIUM-CONTAINING RAW MATERIAL FOR HARDENING WITH ADMIXTURES AND METHOD OF MANUFACTURING LEATHER | 1993 |
|
RU2085591C1 |
Authors
Dates
1996-03-27—Published
1994-04-27—Filed