FIELD: leather industry. SUBSTANCE: chlorine-containing titanium sulfate is dissolved in water, the process takes place till concentration of titanium, sulfate ion and chlorine ion is 80-140 g/l, 180-340 g/l and not more 65 g/l respectively. Thus prepared solution is mixed and cooled, then two-stepped salting out of ammonium sulfatotitanium is carried out. At the first step solid ammonium sulfate is added into solution, its quantity is 30-40 % of total value, rate of salting out is 0.22-0.27 kg/s. At the second step solid ammonium sulfate is added into solution, its quantity being 70-60 % of total value, rate of salting out is 0.6-0.07 kg/s. EFFECT: improved efficiency of the method. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCTION OF TITANIUM TANNING AGENT FOR LEATHER | 1994 |
|
RU2057185C1 |
METHOD OF PREPARING TITANIUM TANNING AGENTS FOR SKIN | 1996 |
|
RU2103372C1 |
METHOD FOR PRODUCTION OF TITANIUM TANNING AGENT FOR LEATHER | 1994 |
|
RU2057184C1 |
METHOD OF PREPARING TITANIUM TANNING AGENT FOR LEATHER | 1995 |
|
RU2113492C1 |
TITANIUM TANNING AGENT | 1995 |
|
RU2112809C1 |
METHOD OF PRODUCING MINERAL TANNING AGENT | 2012 |
|
RU2509810C1 |
FILTER MEDIUM | 1995 |
|
RU2104748C1 |
METHOD OF PRODUCING TITANIUM TANNING AGENT | 2012 |
|
RU2484143C1 |
METHOD OF PREPARING TITANIUM HARDENER FROM TITANIUM-CONTAINING RAW MATERIAL FOR HARDENING WITH ADMIXTURES AND METHOD OF MANUFACTURING LEATHER | 1993 |
|
RU2085591C1 |
METHOD OF PROCESSING SPHENE CONCENTRATE | 2009 |
|
RU2394768C1 |
Authors
Dates
1997-04-27—Published
1994-03-05—Filed