FIELD: textile industry. SUBSTANCE: a single yarn is formed from fibers (length is 30-40 mm) at twisting coefficient = 34.8-36.4 followed by its reeling on the packer at density = 0.28-0.32 g/cm3. The latter is treated with stimulating agent as steam or the preparation based on paraffin emulsion. Packer treatment with steam is carried out at 75-85 C for 30-45 min. EFFECT: improved method of yarn production. 3 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
YARN FOR FABRICS AND KNITTING WARE (VERSIONS), METHOD OF MANUFACTURING THEREOF, FABRIC AND KNITTING CLOTH | 1996 |
|
RU2090673C1 |
YARN FOR WOVEN AND KNITTED WARE AND METHOD OF MANUFACTURING THEREOF | 1995 |
|
RU2098526C1 |
TWIST YARN FOR WOVEN AND KNITTED FABRIC AND TWIST YARN MANUFACTURE METHOD | 2000 |
|
RU2170782C1 |
SEMIFINISHED PRODUCT FOR SPINNING PRODUCTION, METHOD OF ITS MANUFACTURE AND DEVICE FOR ITS ACCOMPLISHMENT | 1993 |
|
RU2057824C1 |
YARN FOR WEAVES AND KNITWEAR, METHOD OF MANUFACTURING THEREOF, AND FABRIC AND KNITTED CLOTH | 1996 |
|
RU2099450C1 |
YARN FOR WOVEN AND KNITTED ARTICLES (VERSIONS) | 1995 |
|
RU2101398C1 |
WET SPINNING YARN PRODUCING METHOD | 1999 |
|
RU2145650C1 |
METHOD FOR PRODUCING COMBINED THREAD IN TWISTER WITH HOLLOW SPINDLE | 1998 |
|
RU2135652C1 |
TEXTILE YARN FOR MANUFACTURE OF ARTICLES TO BE USED FOR PROTECTING FROM OPEN FIRE | 2004 |
|
RU2286410C2 |
METHOD OF PREPARATION OF DOUBLE TWISTED WARP YARN FOR WEAVING | 0 |
|
SU1751232A1 |
Authors
Dates
1996-05-27—Published
1993-06-30—Filed