FIELD: production of cardboard. SUBSTANCE: starch is preliminary treated by urea, its quantity being 1-16 % of starch mass, the process is carried out at 80-90 C within 4-5 h. Thus obtained product is mixed with aqueous solution of hydrogen peroxide and is allowed to stand at 60-70 C within 1-2 h. Quantity of hydrogen peroxide in mixture is 0.35-1.0 % of mass of starch product. EFFECT: improves efficiency of method. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCTION OF WATER-SOLUBLE MODIFIED STARCH | 1992 |
|
RU2057142C1 |
METHOD FOR PRODUCTION OF PHOSPHORYLATED STARCH | 1992 |
|
RU2057143C1 |
FINELY DISPERSED STARCH-CONTAINING DISPERSIONS OF POLYMERS, METHOD OF OBTAINING THEREOF AND APPLICATION THEREOF AS GLUING MEANS IN PAPER PRODUCTION | 2010 |
|
RU2523533C2 |
POLYMER COMPOSITION, USE THEREOF AND SURFACE SIZING | 2017 |
|
RU2733729C2 |
PROCESS FOR MANUFACTURING FLUID FOOD PRODUCTS PACKING BOARD | 0 |
|
SU1807147A1 |
METHOD OF PRODUCING PHOSPHORATED STARCH | 0 |
|
SU1643556A1 |
METHOD OF PRODUCING DYE WITH STARCH COMPONENT | 2014 |
|
RU2595691C2 |
METHOD OF PRODUCING A SIZING AGENT COMPOSITION, A SIZING AGENT COMPOSITION AND USE THEREOF | 2016 |
|
RU2706306C1 |
METHOD FOR OBTAINING FOOD COLORING STARCH-CONTAINING ADDITIVES | 2017 |
|
RU2656659C1 |
SYNTHETIC GLUE AND METHOD OF PREPARATION THEREOF | 2001 |
|
RU2181369C1 |
Authors
Dates
1996-06-10—Published
1994-08-04—Filed