FIELD: internal-combustion engines. SUBSTANCE: in producing semiconductor component of spark plug, compound composed of copper and chromium oxide is applied to its working surface; semiconductor component is made of chromium oxide and bismuth oxide in the following proportion, mass percent: Cr2O3 - 99.0-99.9; Bi2O3 - 1.0-0.1; component is annealed at 1640-1660 C; annealing cycle takes 8 h; compound containing copper and chromium oxide and applied to working surface of semiconductor component is burned at 1180-1120 C for 10-20 min. EFFECT: facilitated procedure. 2 tbl
| Title | Year | Author | Number | 
|---|---|---|---|
| METHOD FOR MANUFACTURING A SEMICONDUCTOR ELEMENT OF A SPARK PLUG | 2022 | 
 | RU2779289C1 | 
| GLASS-CONTAINING SEALING COMPOUND FOR SPARK PLUGS | 1991 | 
 | SU1825261A1 | 
| SEMICONDUCTOR SPARK-PLUG | 1991 | 
 | RU2007004C1 | 
| SEMICONDUCTOR SPARK-PLUG FOR GAS-TURBINE | 1991 | 
 | RU2028023C1 | 
| SPARKING PLUG | 1989 | 
 | SU1720459A1 | 
| SEMICONDUCTOR SPARK-PLUG FOR GAS-TURBINE ENGINE | 1989 | 
 | SU1713399A1 | 
| SEMICONDUCTOR SPARK PLUG | 1993 | 
 | RU2063098C1 | 
| PIEZOELECTRIC CERAMIC MATERIAL | 1998 | 
 | RU2139840C1 | 
| PIEZOELECTRIC CERAMIC MATERIAL | 1993 | 
 | RU2081093C1 | 
| CAPACITOR-TYPE IGNITION SYSTEM OF GAS-TURBINE ENGINE | 1995 | 
 | RU2106518C1 | 
Authors
Dates
1996-06-27—Published
1993-03-01—Filed