FIELD: various industries. SUBSTANCE: starting fiber composed of polyacrylonitrile, copolymer or polyvinylchloride thereof is treated with modifying agent during circulation at 20-90 C. The whole is squeezed out to obtain increased amount of working solution of 50-200 wt% and heated at 100-140 C for 10-120 min. EFFECT: more efficient preparation process. 4 cl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCTION OF ION EXCHANGE POLYACRYLONITRILE FIBER | 1993 |
|
RU2044748C1 |
METHOD OF MANUFACTURING CHEMISORPTION CARBOXYL-CONTAINING FIBER | 1996 |
|
RU2102544C1 |
METHOD OF OBTAINING ANION-EXCHANGE FIBRE MATERIAL, CAPABLE OF EXTRACTING CHROMIUM (VI) | 2008 |
|
RU2368711C1 |
0 |
|
SU332148A1 | |
METHOD OF MANUFACTURING ION-EXCHANGE POLYACRYLONITRILE FIBER (OPTIONS) | 2004 |
|
RU2262557C1 |
METHOD OF FIBROUS IONITE PRODUCING | 1992 |
|
RU2101306C1 |
METHOD TO PRODUCE A GRAFTED COPOLYMER OF POLYCAPROAMIDE | 2001 |
|
RU2217443C2 |
METHOD OF PRODUCING ION-EXCHANGE POLYACRYL-NITRYL FIBRE | 0 |
|
SU1068556A1 |
METHOD OF CATIONIC DYE SALTS PREPARING | 1992 |
|
RU2011669C1 |
METHOD OF CHEMISORPTION FIBERS MODIFICATION | 1990 |
|
SU1750275A1 |
Authors
Dates
1996-09-27—Published
1993-07-12—Filed