FIELD: detergents. SUBSTANCE: method involves neutralization of zeolite NaA suspension by continuous blowing foam gases through its that contain 6-12% carbon dioxide. Ratio gas : zeolite suspension = 1:(2-4) by volume. Value pH of zeolite suspension after neutralization is 10.0-11.5, cation-exchange capacity of zeolite NaA is 140-180 mg/g (by CaO). EFFECT: improved method of neutralization.
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD OF PREPARING GRANULATED SYNTHETIC ZEOLITE-CONTAINING SYNTHETIC DETERGENT COMPONENT | 2002 |
|
RU2230779C1 |
| METHOD OF DETERMINING ZINC IN WATER | 1998 |
|
RU2125724C1 |
| METHOD FOR PRODUCING ZEOLITES | 1997 |
|
RU2111166C1 |
| ORGANOMINERAL FERTILIZERS PRODUCTION PROCESS | 2001 |
|
RU2185353C1 |
| METHOD OF DETERMINING MICROAMOUNTS OF TOTAL CHROMIUM IN WATER | 1997 |
|
RU2137112C1 |
| METHOD FOR PRODUCTION OF WATER GLASS | 1993 |
|
RU2057069C1 |
| METHOD OF PRODUCING ZEOLITE NaA AS DETERGENT | 2015 |
|
RU2603800C1 |
| METHOD FOR TREATMENT OF SEWAGE POLLUTED WITH CR (VI) | 2001 |
|
RU2233245C2 |
| METHOD OF SODIUM ALUMINISILICATE PRODUCING | 1992 |
|
RU2044689C1 |
| METHOD OF PRODUCTION OF THE CHEMICALLY DEPOSITED CHALK | 2006 |
|
RU2312065C1 |
Authors
Dates
1996-10-10—Published
1994-01-10—Filed