FIELD: technology of inorganic compounds and preparation of pure scandium compounds. SUBSTANCE: scandium containing concentrate is dissolved in mineral acid, solution is treated with sulfuric acid to concentration of 260-400 g/cu. dm in the solution. The precipitate is separated from the solution, washed and dissolved in water. Low-soluble scandium compounds such as scandium hydroxide and/or oxalate are precipitated. EFFECT: more efficient preparation process. 3 cl, 2 ex, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF CONCENTRATING SCANDIUM DERIVED FROM WASTES OF WOLFRAMITE CONCENTRATE PROCESSING | 1993 |
|
RU2069180C1 |
METHOD OF PROCESSING SCANDIUM-CONTAINING SOLUTIONS | 2001 |
|
RU2196184C2 |
SCANDIUM OXIDE PREPARATION PROCESS | 2003 |
|
RU2257348C1 |
METHOD OF THORIUM RECOVERY AND CONCENTRATION FROM PROCESS SOLUTIONS | 2001 |
|
RU2207393C1 |
METHOD FOR PREPARATION OF SCANDIUM OXIDE FROM SCANDIUM-CONTAINING CONCENTRATES | 2018 |
|
RU2669737C1 |
METHOD FOR SULPHURIC ACID PROCESSING OF SCANDIUM-CONTAINING RAW MATERIALS | 2023 |
|
RU2806940C1 |
OBTAINING SCANDIUM-CONTAINING CONCENTRATE AND FOLLOWING REMOVING THE SCANDIUM OXIDE OF HIGH PURITY | 2016 |
|
RU2647398C2 |
METHOD OF SCANDIUM EXTRACTION FROM TITANIUM TETRACHLORIDE PRODUCTION WASTE | 1993 |
|
RU2068392C1 |
METHOD OF A COMPLEX PROCESSING OF A METALLURGICAL SCRAP | 2003 |
|
RU2258752C2 |
METHOD FOR RECOVERING AND DECONTAMINATING RADIOACTIVE INDUSTRIAL PRODUCTS AND/OR INDUSTRIAL WASTES | 2001 |
|
RU2205461C2 |
Authors
Dates
1996-11-20—Published
1993-07-23—Filed