FIELD: mining industry. SUBSTANCE: composition contains 77.0-79.5 wt % ammonium nitrate, 5.0-10.0 wt % trotyl, 5.0-7.5 wt % kerogene, and water. Composition is prepared by a standard process with the aid of charge-mixing machines. Composition is characterized with density 1.36-1.38 g/cu.cm, detonation rate 3200-3500 m/s, and crystallization temperature 60- 65 C. EFFECT: improved performance characteristics suitable for open pit mining.
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MANUFACTURING AQUATRINITROTOLUENE TYPE EXPLOSIVE | 1998 |
|
RU2144524C1 |
METHOD OF CHARGING OF DESCENDING BLAST HOLES WITH HOT-FLOWING WATER-CONTAINING EXPLOSIVES | 1994 |
|
RU2100773C1 |
METHOD OF PREPARING WATER-CONTAINING EXPLOSIVE | 1998 |
|
RU2145589C1 |
METHOD OF PREPARING WATER-CONTAINING EXPLOSIVE | 1998 |
|
RU2138468C1 |
PROCESS OF LOADING OF DOWNGOING HOLES WITH WATER-CARRYING EXPLOSIVES (VERSIONS) | 1999 |
|
RU2146037C1 |
METHOD FOR ROCK BREAKING | 1992 |
|
RU2043497C1 |
METHOD FOR PRODUCTION OF WATER-CONTAINING EXPLOSIVES | 2000 |
|
RU2204544C2 |
WATER-CONTAINING EXPLOSIVE | 1997 |
|
RU2118307C1 |
EXPLOSIVE MIXTURE (VARIANTS) | 2004 |
|
RU2253643C1 |
A WATER-CONTAINING BLASTING EXPLOSIVE OF THE HEIGHTENED EXPLOSIVE EFFICIENCY | 2001 |
|
RU2265003C2 |
Authors
Dates
1997-01-20—Published
1992-03-13—Filed