FIELD: manufacture of building materials. SUBSTANCE: formulation contains (in wt %): urea-formaldehyde resin, 20-35; phosphoric acid, 2.0-3.0; surfactant (blowing agent), 0.4-0.5; carbonation modifier with 60- 85% humin acids, 0.4-0.6; water, the balance. Aqueous solution of resin, surfactant, and carbonation modifier is foamed with compressed air, then phosphoric acid is added to form low toxic foam plastic. EFFECT: reduced toxicity of product. 1 tbl, 3 ex
Title | Year | Author | Number |
---|---|---|---|
MIXTURE FOR OBTAINING FOAM PLASTIC | 2006 |
|
RU2326141C1 |
RAW MIXTURE FOR MAKING HEAT INSULATING OBJECTS BASED ON FOAM PLASTIC | 2008 |
|
RU2376329C2 |
RAW MIX FOR HEAT-INSULATION MATERIALS AND A METHOD FOR PREPARATION THEREOF | 2002 |
|
RU2237033C2 |
PROCESS FOR PREPARING FOAMED PLASTIC | 1992 |
|
RU2039768C1 |
COMPOSITION FOR PREPARING PLASTIC FOAM AND METHOD OF PREPARATION THEREOF | 1992 |
|
RU2091407C1 |
HEAT-INSULATING POLYMERIC MATERIAL AND METHOD FOR ITS PREPARING | 2004 |
|
RU2277518C2 |
PROCESS FOR PREPARING CARBIDE-FORMALDEHYDE PLASTIC FOAM | 1994 |
|
RU2082731C1 |
COMPOSITION FOR MAKING PLASTIC FOAMS | 1997 |
|
RU2123018C1 |
POLYMER COMPOSITION FOR FOAM PLASTIC | 2015 |
|
RU2593160C1 |
COMPOSITION FOR FOAMED PLASTIC MATERIAL | 1992 |
|
RU2072375C1 |
Authors
Dates
1997-02-27—Published
1994-02-03—Filed