FIELD: construction. SUBSTANCE: mix for preparing phosphate binder comprises (wt%): 20.25-26.47 othophosphoric acid; 70-75.0, metal phosphatization waste; and water balance. Ultimate compression strength 19-24 Mpa and hardening temperature: 20 C. EFFECT: improved properties of the phosphate binder. 1 tbl