FIELD: rubber industry. SUBSTANCE: method involves mixing the composition based on butadiene-containing rubber and its vulcanization under pressure. After vulcanization mixture is subjected for additional treatment at 225-300 C for 3-10 h. EFFECT: high conductivity and thermostability, retained properties. 5 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING RUBBER MIX | 1994 |
|
RU2087494C1 |
METHOD OF PREPARATION OF REGENERATE | 1994 |
|
RU2087493C1 |
METHOD OF PRODUCING ELECTROCONDUCTIVE ELASTOMERIC MATERIAL | 2011 |
|
RU2472813C1 |
TONER PREPARATION METHOD | 1997 |
|
RU2117974C1 |
METHOD OF PRODUCING COMPOSITE POLYMER MEMBRANE FOR SEPARATION OF CARBON DIOXIDE FROM GAS MIXTURES | 1998 |
|
RU2146169C1 |
METHOD OF RADIO-OPAQUE COMPOSITION PRODUCING | 1993 |
|
RU2083609C1 |
VULCANIZABLE RUBBER STOCK | 0 |
|
SU1016324A1 |
METHOD OF REVEALING INTERNAL DEFECTS OF THERMOSET PRODUCTS | 1994 |
|
RU2088910C1 |
METHOD FOR MAKING POROUS PRODUCTS OF REFRACTORY MATERIALS | 1997 |
|
RU2171732C2 |
VULCANIZABLE RUBBER STOCK | 0 |
|
SU1014848A1 |
Authors
Dates
1997-04-27—Published
1994-02-04—Filed