FIELD: chemistry.
SUBSTANCE: method of producing electroconductive elastomeric composite material based on general or special-purpose rubber involves mixing 100 pts.wt rubber, 10-13 pts.wt vulcanising group, 20-25 pts.wt plasticiser, 10-25 pts.wt graphite and 25-60 pts.wt electroconductive technical carbon. Pressure curing is then carried out. After curing, the material is subjected to swelling in an organic solvent until achieving equilibrium swelling index and then held for 1 hour at 100-120°C after complete removal of solvent.
EFFECT: disclosed material has high electroconductivity.
2 tbl, 26 ex
Title | Year | Author | Number |
---|---|---|---|
RUBBER MIXTURE FOR MAKING OIL-SWELLING PRODUCTS | 2021 |
|
RU2765950C1 |
FROST-RESISTANT RUBBER MIXTURE FOR MANUFACTURE OF RUBBER PRODUCTS WITH WIDE OPERATING TEMPERATURE RANGE | 2023 |
|
RU2807833C1 |
FIREPROOF RUBBER MIXTURE | 2012 |
|
RU2522627C2 |
COMPOSITE MATERIAL FOR FIREARMS TRAUMATIC PROPELLANT BULLETS | 2014 |
|
RU2553908C1 |
POLYMER COMPOSITIONS CONTAINING NANOTUBES | 2016 |
|
RU2669090C2 |
RUBBER MIXTURE | 2023 |
|
RU2813595C1 |
RUBBER COMPOUND BASED ON NITRILE RUBBER | 2021 |
|
RU2790668C1 |
ANTIFOULING RUBBER COMPOSITION | 2023 |
|
RU2811806C1 |
RUBBER MIXTURE | 2020 |
|
RU2751316C1 |
ELASTOMERIC COMPOSITION | 2018 |
|
RU2680508C1 |
Authors
Dates
2013-01-20—Published
2011-10-20—Filed