FIELD: chemical industry. SUBSTANCE: zeolite NaA is treated with cobalt-containing solution resulting from deposition of cobalt hydroxide during hydrochemical treatment of cobalt-nickel concentrate to neutral reaction of liquid phase. The product is filtered, washed, dried and calcined at 1000-1100 C for 3 or 4 hours. Pigment comprises 4.0-4.5 wt% $$$, has crystalline nephelinic structure with main lines on X-ray diffraction pattern and color characteristics of standard cobalt aluminate ("cobalt blue"). EFFECT: more efficient preparation process.
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD OF PRODUCING CERAMIC ALUMINIUM-COBALT OXIDE PIGMENT BASED ON NANO-SIZED MESOPOROUS SYNTHETIC XONOTLITE | 2010 |
|
RU2493185C2 |
| METHOD OF PREPARING THERMOSENSITIVE REVERSIBLE PIGMENT | 1999 |
|
RU2154659C1 |
| METHOD OF RECOVERY OF COBALT FROM COBALT-CONTAINING MATERIAL | 1998 |
|
RU2127326C1 |
| METHOD OF PREPARING ZEOLITE (NA,LI)F MONOCRYSTALS | 1986 |
|
RU1450409C |
| NOZZLE | 1992 |
|
RU2036314C1 |
| METHOD OF SYNTHESIS OF CARBAMIDOFORMALDEHYDE OLIGOMERIC ADDITIVE TO CARBAMIDE RESINS | 1992 |
|
RU2050372C1 |
| AEROSOL FERTILIZER FOR NON-ROOT | 1996 |
|
RU2106328C1 |
| METHOD OF RECOVERING OSMIUM FOR ION-EXCHANGE RESIN | 1998 |
|
RU2131939C1 |
| PORTABLE FILTER PRESS-TYPE ELECTROLYZER FOR PRODUCING OXYGEN AND HYDROGEN | 1993 |
|
RU2049157C1 |
| METHOD FOR PRODUCTION OF MONOMETHYL HOMOLOGS OF CYCLIC SULFONE BUTADIENE-1,3 (SULFOLENE-3) | 1995 |
|
RU2065858C1 |
Authors
Dates
1997-05-27—Published
1993-06-15—Filed