FIELD: production of film being used for packing of food products and drugs. SUBSTANCE: proposed composition contains 100 mass parts of polyvinyl chloride, 1-3 mass parts of calcium stearate, 0.3-1.5 mass parts of zinc stearate, 2-3 mass parts of soya oil affected by epoxydation, 0.2-0.3 mass parts of glycerine, 2-3 mass parts of titanium dioxide, 0.1-0.2 mass parts of stearine, 0.9-1.1 mass parts of trinonyl phenyl phosphite, 3-6 mass parts of mixture of dioxane alcohols and high boiling ethers thereof, 0.04-0.0 mass parts of reapone. Tensile strength of packing film is increased by 30-40 %, its brittleness temperature is decreased by 6-10 C, shrinkage of said film is decreased by 13-30 % by heating. EFFECT: increased tensile strength, decreases brittleness temperature and shrinkage of desired film. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
COMPOSITION FOR COATING | 1994 |
|
RU2071494C1 |
COMPOSITION ON THE BASE OF POLYVINYL CHLORIDE FOR FOAMED PLASTIC | 1993 |
|
RU2095381C1 |
POLYVINYL CHLORIDE COMPOSITION | 1993 |
|
RU2108352C1 |
POLYMER COMPOSITION | 1993 |
|
RU2045553C1 |
POLYMERIC COMPOSITION FOR ARTISTIC-MOSAIC PLATES | 1994 |
|
RU2081890C1 |
METHOD OF PREPARING AMYLENE OXIDES | 1994 |
|
RU2072995C1 |
ADHESIVE COMPOSITION (VARIANTS) | 1996 |
|
RU2114145C1 |
HERMETIC COMPOSITION | 1996 |
|
RU2101316C1 |
SEALING COMPOSITION | 1992 |
|
RU2064955C1 |
PHOTOPOLYMERIZING COMPOSITION TO MANUFACTURE NET STENCILS | 1995 |
|
RU2078365C1 |
Authors
Dates
1997-07-10—Published
1994-02-14—Filed