FIELD: non-ferrous metallurgy, instrument making. SUBSTANCE: method involves production of alloy followed by its deformation with more than 80 % compression and by annealing. Said alloy is prepared of mixture which contains 24-32 mass % of Cu, 16-20 mass % of Au, 10-18 mass % of Ag and Pd. Said annealing is carried out at temperature which is lower than critical ordering temperature, heating rate being not more 30 C/min. EFFECT: improved efficiency of the method.
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MANUFACTURE OF MATERIAL FOR WEAK- CURRENT CONTACTS MADE FROM PALLADIUM-BASED ORDERED ALLOY | 2002 |
|
RU2217524C1 |
METHOD OF MANUFACTURING RESISTIVE MATERIAL FROM Cu-Pd-BASED ORDERING ALLOY | 2016 |
|
RU2643733C2 |
METHOD OF THERMAL TREATMENT OF CONTACT PAIR FROM GOLD-COPPER ALLOY ZlM-80 FOR ELECTRIC LOW-CURRENT SLIDING CONTACTS | 2019 |
|
RU2716366C1 |
METHOD FOR HYDRAULICALLY EXTRUDING PRECISE SHAPES OF NON-FERROUS AND NOBLE METAL ALLOYS | 1995 |
|
RU2084304C1 |
WHITE-GOLD ALLOY | 1998 |
|
RU2135618C1 |
METHOD FOR PRODUCTION OF COPPER LONG BLANK | 1997 |
|
RU2106215C1 |
METHOD OF CONTROLLING TEMPERATURE ALONG STRIP WIDTH AT HEAT TREATMENT | 1993 |
|
RU2071991C1 |
PLATINUM-BASED ALLOY | 1995 |
|
RU2085606C1 |
METHOD OF PROCESSING BRASS TAPE | 1994 |
|
RU2092609C1 |
JEWELRY ALLOY BASED ON HALLMARK 585 GOLD | 1999 |
|
RU2170280C1 |