FIELD: powder metallurgy, in particular, production of antifriction parts from iron-based materials. SUBSTANCE: composition is characterized in that aluminum powder is added into powder material. Composition contains the following components, % by weight: aluminum 0.03-1.4; copper 1-20; graphite 0.5-5.0; iron the balance. Aluminum and copper are taken in the ratio of 0.03-0.07% by weight. EFFECT: increased efficiency and improved quality of antifriction parts. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
COMPOSITION OF MIXTURE FOR MANUFACTURE OF CERMET SEALING MATERIALS | 1998 |
|
RU2157857C2 |
CHARGE FOR ANTIFRICTION COMPOSITE MATERIAL ON BASIS OF ALUMINIUM AND SINTERED ANTIFRICTION COMPOSITE MATERIAL ON BASIS OF ALUMINIUM, RECEIVED WITH ITS APPLICATION | 2007 |
|
RU2359051C2 |
SINTERED COMPOSITE MATERIAL BASED IN COPPER | 1997 |
|
RU2112068C1 |
ELECTRIC BRUSH MANUFACTURING PROCESS | 1994 |
|
RU2088007C1 |
ANTIFRICTION FILLED COMPOSITION AND METHOD OF ITS PREPARING | 2000 |
|
RU2181128C1 |
METHOD OF MANUFACTURING ARTICLES FROM METAL POWDERS | 1989 |
|
RU1750115C |
METHOD OF PRODUCTION OF ALUMINIUM ALLOYS WITH DISPERSION HARDENING | 1993 |
|
RU2083321C1 |
CURRENT-COLLECTOR MATERIAL | 1992 |
|
RU2049687C1 |
ANTIFRICTION COMPOSITION | 1999 |
|
RU2153107C1 |
POROUS MATERIAL FOR FILTERS | 1997 |
|
RU2124965C1 |
Authors
Dates
1997-07-27—Published
1994-09-21—Filed