FIELD: polymeric materials. SUBSTANCE: for producing thermoweldable films (thickness is 100 mm) and sheets (100 mm) the following composition is used, mas. p. : polypropylene (isotacticity index is above 90) 36.8-46.0; xylene-insoluble at room temperature polyethylene 15-20, and amorphous copolymer of ethylene with propylene containing 40-70% ethylene 37.2-44.2. Ratio of true viscosity value in tetrahydronaphthalene at 135 C of the indicated components that are insoluble and soluble in xylene at room temperature = 0.8-1.2. EFFECT: high elastomeric properties of composition. 3 cl, 5 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF COATING METAL PIPES, POLYOLEFIN COMPOSITION, FILM, TAPE OR STRIP | 1994 |
|
RU2144051C1 |
POLYMER COMPOSITION, METHOD FOR ITS PRODUCTION AND COMPOSITE MATERIAL | 1990 |
|
RU2092502C1 |
FILM OR SHEET MATERIAL, FILM OR SHEET PRODUCT (VARIANTS) | 1994 |
|
RU2124535C1 |
PARTIALLY CROSS-LINKED POLYOLEFIN MIXTURES | 1998 |
|
RU2205846C2 |
PARTIALLY CRYSTALLINE POLYOLEFINIC COMPOSITION AND METHOD OR PREPARATION THEREOF | 1993 |
|
RU2104289C1 |
POLYOLEFINIC COMPOSITION | 1993 |
|
RU2110536C1 |
POLYOLEFIN COMPOSITE AND EMBOSSED SHEET | 1997 |
|
RU2194727C2 |
POLYMER BLEND FOR MOLDING HOLLOW PRODUCTS BY POURING AND SLOW ROTATION OF MOLD | 1997 |
|
RU2186798C2 |
POLYMER COMPOSITION ON BASE OF POLYOLEFINS | 1993 |
|
RU2105777C1 |
METHOD OF REPAIRING PLASTIC COATINGS ON METALLIC PIPES AND REPAIR COATING | 1993 |
|
RU2109787C1 |
Authors
Dates
1997-07-27—Published
1991-02-27—Filed