FIELD: erection and repair of pipe lines. SUBSTANCE: layer of mixture containing calcium oxide of inorganic binder and adhesive is secured on porous nonwoven or woven base of material. Ratio of thicknesses of layers of base and anticorrosive layer of mixture ranges from 1:1 to 1:5. Anticorrosive material wetted with water is tightly wound on surface protected. EFFECT: enhanced efficiency. 2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
AQUEOUS COMPOSITION FILLED WITH HOLLOW MICROSPHERES FOR PREPARING ANTICORROSIVE AND HEAT-INSULATING COVER AND METHOD FOR PREPARING COVER BASED ON THEREOF | 2005 |
|
RU2304156C1 |
METHOD FOR PRODUCTION OF HEAT INSULATION AND FIRE RESISTANT COMBINED POLYMER COATING | 2007 |
|
RU2352601C2 |
METHOD FOR PRODUCTION OF HEAT INSULATION MULTILAYER COMBINED POLYMER COATING (VERSIONS) | 2007 |
|
RU2352467C2 |
METHOD OF PIPELINE CORROSION PROTECTION | 2007 |
|
RU2340830C1 |
METHOD OF REPAIRING CORROSION PROTECTION OF PIPELINE | 2004 |
|
RU2265151C1 |
COILED MASTIC MATERIAL | 2008 |
|
RU2379575C2 |
ROLLED MASTIC MATERIAL ON TEXTILE BASE TAPE IMPREGNATED WITH MASTIC USING ASPHALTIC RESINOUS OLIGOMERS (VERSIONS) | 2010 |
|
RU2458282C2 |
METHOD OF MANUFACTURE OF HEAT-INSULATING MEMBER OF PIPE LINE | 2002 |
|
RU2215233C1 |
METHOD OF FABRICATING PIPELINE INSULATED SLEEVE JOINT | 2007 |
|
RU2341720C1 |
MULTILAYERED INSULATION COATING FOR PIPELINE | 2016 |
|
RU2639257C2 |
Authors
Dates
1997-08-27—Published
1995-03-13—Filed