FIELD: electrodeposition, electrolyte galvanizing. SUBSTANCE: for decrease of mass of carry-over of zinc compounds with coated parts electrolyte contains 25.0-40.0 g/l septiwater zinc sulfate; 140.0- 160.0 g/l ammonium chloride; 0.002-0.004 g/l product of condensation of polyethylenepolyamine, tiocarbide and formaldehyde and 0.4-1.0 g/l polyvinylamin oil acid. EFFECT: decreased mass of carry-over of zinc compounds. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
ELECTROLYTE FOR ELECTRIC PRECIPITATION OF ZINC-NICKEL ALLOY | 2010 |
|
RU2441107C1 |
ELECTROLYTE FOR ELECTRODEPOSITION OF LUSTROUS ZINC COATINGS | 2024 |
|
RU2820435C1 |
BRIGHT NICKEL ELECTROLYTE | 2021 |
|
RU2769796C1 |
ELECTROLYTE FOR ELECTROCHEMICAL DEPOSITION OF COATINGS NICKEL-BORON | 2008 |
|
RU2357015C1 |
ALKALINE ELECTROLYTE FOR ELECTRODEPOSITION OF ZINC-NICKEL COATINGS | 2013 |
|
RU2511727C1 |
PYROPHOSPHATE CONTAINING ELECTROLYTE FOR DEPOSITING TIN-ZINC ALLOY | 2005 |
|
RU2292408C1 |
SHINNING ZINC-PLATING ELECTROLYTE | 1994 |
|
RU2063481C1 |
ELECTROLYTE FOR SEDIMENTATION OF COMPOSITION COATING NICKEL-COBALT-DIAMOND | 2008 |
|
RU2362843C1 |
ELECTROLYTE FOR DEPOSITION OF ZINC COAT | 2000 |
|
RU2184800C2 |
ELECTROLYTE FOR DEPOSITING IRON COATINGS | 1995 |
|
RU2110622C1 |
Authors
Dates
1997-09-10—Published
1994-12-06—Filed