FIELD: chemistry.
SUBSTANCE: electrolyte contains, g/l: zinc oxide 12-15, caustic soda 100-120, sulfuric nickel 7-17, triethanolamine 40-60, hexamethylenediamine- N,N,N',N'- tetraacetic acid 0.5-2, diglycine 1-3, water to 1 l.
EFFECT: increase of corrosion stability of zinc-nickel coatings, extension of range of working current densities, reduction of ecological load on purification of sewages by application of low-concentrated electrolytes.
2 tbl, 4 ex
Title | Year | Author | Number |
---|---|---|---|
ELECTROLYTE FOR ZINC-NICKEL COATINGS DEPOSITION | 2016 |
|
RU2627319C1 |
ELECTROLYTE FOR ELECTRODEPOSITION OF ZINC-NICKEL COATINGS | 2015 |
|
RU2603526C1 |
METHOD OF APPLYING NICKEL COATING ON STEEL AND COPPER COMPONENTS IN NICKEL PLATING ELECTROLYTE | 2011 |
|
RU2489525C2 |
METHOD OF APPLYING ELECTROCONDUCTIVE PROTECTIVE COATING ON ALUMINIUM ALLOYS | 2023 |
|
RU2817277C1 |
METHOD OF NICKELIZING STEEL, COPPER, AND COPPER ALLOY PARTS | 1996 |
|
RU2089675C1 |
ELECTROLYTE FOR ELECTRODEPOSITION OF TIN-NICKEL COATINGS | 2013 |
|
RU2526656C1 |
METHOD OF PREPARING COATINGS SUITABLE FOR PROTECTION OF STEEL PARTS AGAINST CORROSION | 2000 |
|
RU2177055C1 |
ELECTROLYTE FOR DIRECT NICKEL-PLATING OF ALUMINIUM AND ITS ALLOYS | 1992 |
|
RU2061104C1 |
ELECTROLYTE FOR ELECTRODEPOSITION OF ZINC-IRON COATINGS | 2019 |
|
RU2712582C1 |
ELECTROLYTE TO PRODUCE ZINC-NICKEL COVER | 1992 |
|
RU2036255C1 |
Authors
Dates
2014-04-10—Published
2013-01-09—Filed