FIELD: processing of hubnerite concentrates. SUBSTANCE: mixture which comprises hubnerite concentrate (WO3 25.2 %), sodium sulfate and coke at their mass ratio 10.0:7.3-7.5:0.5-0.6 respectively is affected by caking within 1 h. The process is carried out in closed crucibles without free access of air at 800 C. Thus reduction atmosphere in reaction zone is produced, it results in fact that decomposition degree of hubnerite concentrate is 99.1-99.3 %. EFFECT: improved quality of desired product.
Title | Year | Author | Number |
---|---|---|---|
METHOD OF SYNNERITE PROCESSING | 1995 |
|
RU2078038C1 |
WOLFRAMITE CONCENTRATE PROCESSING METHOD | 2005 |
|
RU2293132C1 |
METHOD OF PROCESSING HUEBNERITE CONCENTRATES | 0 |
|
SU861318A1 |
METHOD FOR TREATMENT OF SEWAGE AND DEVICE FOR ITS EMBODIMENT | 1993 |
|
RU2057080C1 |
METHOD OF ELECTRON BEAM CUTTING | 1991 |
|
RU2088389C1 |
METHOD OF PROCESSING HUBNERITE CONCENTRATES | 0 |
|
SU827399A1 |
METHOD FOR PROCESSING TUNGSTEN CONCENTRATES | 2022 |
|
RU2785560C1 |
METHOD FOR PROCESSING SYNNYRITE INTO POTASSIUM, MAGNESIUM SULPHATES AND ALUMINA | 2020 |
|
RU2749824C1 |
TUNGSTENITE CONCENTRATE PROCESSING METHOD | 2011 |
|
RU2465357C1 |
WIDE-APERTURE PLASMA EMITTER | 1996 |
|
RU2096857C1 |
Authors
Dates
1997-09-27—Published
1995-05-17—Filed