FIELD: metallurgy, in particular, steel continuous casting. SUBSTANCE: method includes successive laying of bricks of safety and working lining of walls and bottom of ladle body and gap with thickness of 0.008-0.12 of ladle bottom diameter between working linings of walls and bottom. Gap is filled with anhydrous mixture of the following composition, vol.%: magnesium sulfate 7-10; finely divided clay 8-10; the balance, magnesite powder. Then, ladle is heated up to 1200 C. At temperature up to 1000 C anhydrous mixture remains in yielding state and does not higher heat expansion of bricks. EFFECT: higher stability of refractory lining of ladles. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF STEEL TEEMING LADLE LINING AND STEEL TEEMING LADLE | 2011 |
|
RU2486989C2 |
STEEL-TEEMING LADLE LINING METHOD | 1998 |
|
RU2138366C1 |
METHOD FOR PREPARING POURING LADLE IN THE PROCESS OF CONTINUOUS STEEL CASTING | 1994 |
|
RU2025202C1 |
STEEL CASTING LADLE | 1996 |
|
RU2095192C1 |
STEEL TEEMING LADLE | 1996 |
|
RU2096129C1 |
STEEL CASTING LADLE | 1995 |
|
RU2092279C1 |
COVER FOR STEEL CASTING LADLE | 1996 |
|
RU2104121C1 |
STEEL CASTING LADLE | 1995 |
|
RU2083324C1 |
METHOD OF POURING LADLE LINING MANUFACTURING | 2013 |
|
RU2558703C2 |
TUNDISH | 2000 |
|
RU2167030C1 |
Authors
Dates
1997-10-10—Published
1995-07-20—Filed