FIELD: manufacture of fine crystalline corundum. SUBSTANCE: according to first variant, fine crystalline corundum is prepared by thermocouple treatment of aluminium hydroxide at 350-400 C and pressure of 30-40 atm in the presence of 1-20 wt % additive such as mechanically activated aluminium oxide or fine crystalline corundum prepared by thermocouple treatment of mechanically activated aluminium hydroxide. According to second variant, aluminium hydroxide, in combination with additive such as 1-20 wt % aluminium oxide, is subjected to mechanical treatment and the mechanically treated mixture is then subjected to thermocouple treatment at 350-400 C and pressure of 30-400 atm. EFFECT: more efficient preparation process. 3 cl, 3 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING FINE CRYSTALLINE CORUNDUM | 1996 |
|
RU2092438C1 |
METHOD OF PREPARING FINE CRYSTALLINE CORUNDUM | 1999 |
|
RU2167817C2 |
METHOD FOR PRODUCING BARIUM SULFATE | 1996 |
|
RU2109685C1 |
METHOD OF PREPARING FINE-CRYSTALLINE NONALLOYED AND ALLOYED YTTRIUM-ALUMINUM GARNET | 1998 |
|
RU2137867C1 |
METHOD OF PREPARING FINE-GRAINED CORUNDUM | 2002 |
|
RU2229441C1 |
METHOD OF MANUFACTURING CORUNDUM-BASED ABRASIVE FLOUR GRAIN | 2005 |
|
RU2321542C2 |
METHOD FOR PRODUCTION OF SINGLE CRYSTALS OF POTASSIUM AND NIOBIUM SILICATE | 1994 |
|
RU2093616C1 |
METHOD OF OBTAINING FINE CRYSTALLINE CORUNDUM | 2007 |
|
RU2340557C2 |
FINE-CRYSTALLINE ALPHA-ALUMINA PRODUCTION PROCESS | 2004 |
|
RU2257346C1 |
METHOD OF PRODUCING ALUMINIUM ALPHA-OXIDE | 0 |
|
SU1477682A1 |
Authors
Dates
1997-10-20—Published
1996-05-22—Filed