FIELD: manufacture of fine crystalline corundum. SUBSTANCE: aluminium hydroxide is subjected to mechanical activation and then thermocouple treatment at temperatures from 350 to 450 C and water vapor pressure from 30 to 400 C. EFFECT: more efficient preparation method. 14 cl, 1 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING FINE CRYSTALLINE CORUNDUM | 1996 |
|
RU2093464C1 |
METHOD OF PREPARING FINE CRYSTALLINE CORUNDUM | 1999 |
|
RU2167817C2 |
METHOD OF PREPARING FINE-GRAINED CORUNDUM | 2002 |
|
RU2229441C1 |
METHOD OF OBTAINING FINE CRYSTALLINE CORUNDUM | 2007 |
|
RU2340557C2 |
METHOD OF OBTAINING FINE CRYSTALLINE ALLOYED LANTHANUM ALUMINATE | 2006 |
|
RU2340558C2 |
METHOD OF PREPARING FINE-CRYSTALLINE NONALLOYED AND ALLOYED YTTRIUM-ALUMINUM GARNET | 1998 |
|
RU2137867C1 |
METHOD OF PRODUCING A SMALL-CRYSTALLINE ALUMINATE OF MAGNESIUM | 2016 |
|
RU2630112C1 |
METHOD FOR PRODUCING BARIUM SULFATE | 1996 |
|
RU2109685C1 |
METHOD OF MANUFACTURING CORUNDUM-BASED ABRASIVE FLOUR GRAIN | 2005 |
|
RU2321542C2 |
Authors
Dates
1997-10-10—Published
1996-03-06—Filed