FIELD: steel working. SUBSTANCE: composition containing (in wt %) 50-65 phosphoric acid, 3.5-7.5 magnesium oxide, 1.4-3.2 aluminum hydroxide, 0.3-3.9 boric acid, and water is applied onto electric anisotropic steel to form coating with high corrosion immunity and improved physico-mechanical characteristics. EFFECT: increased lifetime of electric steel under high humidity conditions. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
COMPOSITION FOR MANUFACTURING ELECTRICALLY INSULATING COATING | 1995 |
|
RU2098393C1 |
COMPOSITION FOR PREPARING ELECTROINSULATING COATING | 1996 |
|
RU2152456C2 |
ELECTRIC INSULATING COMPOSITION | 1999 |
|
RU2158032C1 |
WATER-SOLUBLE COMPOSITION FOR INSULATING COATING OF ELECTRICAL STEEL | 2001 |
|
RU2208853C1 |
ELECTRIC INSULATION COMPOSITION | 1996 |
|
RU2113026C1 |
COMPOSITION FOR RECEIVING OF ELECTRICAL INSULATING COATING | 2007 |
|
RU2360033C2 |
COMPOUND FOR PRODUCING INSULATING COATING | 1997 |
|
RU2127921C1 |
INSULATING COATING COMPOUND | 2001 |
|
RU2207640C2 |
COMPOSITION FOR PREPARING ELECTROINSULATING COATING | 1996 |
|
RU2117345C1 |
METHOD OF PREPARING ELECTROINSULATING COATING | 1997 |
|
RU2122603C1 |
Authors
Dates
1997-11-27—Published
1996-01-10—Filed