FIELD: insulating materials. SUBSTANCE: method involves preliminary mixing and thorough stirring at 50 C the following components, mas. p. p.: product of condensation of tetrabromodiphenylolpropane with epichlorohydrin melted at temperature C 15-25; epoxy diane resin 35-45; product of condensation of dicarboxylic oligodiethylene glycol sebacate with epoxy diane resin 15-25; product of epichlorohydrin dehydrochlorination with water 15-25; finely dispersed aluminium hydroxide 30-54 and preparing the first component; isomethyltetrahydrophthalic anhydride 35-55 is mixed with 2,4,6-tris-(dimethylaminomethyl)-phenol 0.05-0.25 and the second component is obtained. Then the first component is mixed with the second component taken at stoichiometric amount. The obtained compound is used for making members working at (-60)-(+105) C. EFFECT: improved method of producing. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
SELF-EXTINGUISHING COMPOUND | 1992 |
|
RU2041895C1 |
INSULATION COMPOUND PREPARATION METHOD | 2003 |
|
RU2247752C1 |
CURRENT-CONDUCTING ADHESIVE COMPOSITION | 2005 |
|
RU2308105C1 |
EPOXY COMPOSITION | 2007 |
|
RU2345106C1 |
EPOXY BINDER FOR PRODUCING SELF-EXTINGUISHING FIBERGLASSES BY PULTRUSION METHOD | 2016 |
|
RU2614701C1 |
EPOXIDE COMPOUND USED FOR GLASS-REINFORCED PLASTICS | 2006 |
|
RU2355722C2 |
EPOXY COMPOUND FILLED WITH BIOGENIC SILICA | 2018 |
|
RU2705956C1 |
METHOD OF PRODUCING ELECTRIC ITNSULATION COMPOUND | 0 |
|
SU1470748A1 |
NOVEL CATALYSTS WITH STABILISING EFFECT FOR EPOXY COMPOSITIONS | 2014 |
|
RU2559492C1 |
EPOXIDE GLUE COMPOSITION | 2007 |
|
RU2368636C2 |
Authors
Dates
1997-12-20—Published
1993-02-18—Filed