FIELD: rolling of flattened belt, mainly with width to thickness ratio more than 20. SUBSTANCE: method of making belt comprises steps of symmetrically rolling it with tension and then non- symmetrically rolling with tension at unmatched velocities of working rolls. At first step rolling is realized at deformation degree up to 50 %. At second step unmatched degree of roll velocity values is set according to expression V1/V2=1+(0.5-2.5)$$$/100, where V1 and V2 - velocity values of driving and driven rolls of stand respectively, $$$ - percentage reduction value,%. EFFECT: enhanced efficiency. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MANUFACTURING REINFORCING MATERIAL | 1995 |
|
RU2096101C1 |
METHOD OF PRODUCTION OF STRIPS FROM HIGH-CARBON AND ALLOY STEELS | 2023 |
|
RU2795066C1 |
METHOD FOR MAKING BELTS | 2001 |
|
RU2218216C2 |
METHOD FOR ROLLING HARD-TO-FORM STRIPS WITH PROFILE VARIABLE ALONG ITS LENGTH | 2003 |
|
RU2243832C1 |
COLD ROLLING METHOD FOR CARBON STRIP STEEL AND RELATED MILL | 2007 |
|
RU2354465C1 |
STRIP STEEL COLD ROLLING METHOD | 2004 |
|
RU2254944C1 |
METHOD OF MAKING HIGH-ACCURACY MANIFOLD SECTIONS | 1996 |
|
RU2090273C1 |
METHOD FOR MAKING STEEL STRIPS FOR MAGNETIC SCREENS | 2002 |
|
RU2223334C2 |
STRIP FOR MAKING KINESCOPES | 2002 |
|
RU2223335C2 |
METHOD FOR CONTROL OF TEMPERATURE PROFILE OF MILL ROLLS | 1997 |
|
RU2115494C1 |
Authors
Dates
1997-12-27—Published
1996-08-23—Filed