FIELD: chemical industry, inorganic chemistry. SUBSTANCE: method involves preparing suspension of calcium hydroxide with phosphoric acid which is added by drops to pH = 9-11. After filtration and drying product is subjected for double processing in the presence of hydroxyl-containing component taken at amount 10-12 wt.-% of product weight at 600-700 C for 20-30 min and at 1000-1400 C for 1-4 h. Calcium, strontium, zirconium, aluminium hydroxides were used as hydroxyl-containing component. The end product is used as bioactive ceramics in stomatology and orthopedics. EFFECT: improved quality of product. 2 cl, 7 dwg, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING AMORPHOUS TRICALCIUM PHOSPHATE | 2011 |
|
RU2478570C2 |
METHOD OF PRODUCING AMORPHOUS TRICALCIUM PHOSPHATE | 2019 |
|
RU2730456C1 |
METHOD FOR PRODUCTION OF HYDROXYL APATITE | 1993 |
|
RU2088521C1 |
METHOD OF PRODUCING AMORPHOUS TRICALCIUM PHOSPHATE | 2018 |
|
RU2691051C1 |
METHOD OF PREPARING CALCIUM HYDROXYL APATITE | 1996 |
|
RU2098350C1 |
HYDROTHERMAL METHOD FOR OBTAINING A BIOREABSORBED CERAMIC MATERIAL | 2018 |
|
RU2678812C1 |
METHOD FOR PRODUCING MATERIAL FOR MAKING BONE IMPLANT | 1996 |
|
RU2108069C1 |
PROCESS FOR PRODUCTION OF POTASSIUM HYDROXYLAPATITE | 1992 |
|
RU2014846C1 |
METHOD OF TREATING MAXILLOFACIAL AREA DEFECTS | 1996 |
|
RU2122365C1 |
ANTICORROSIVE PIGMENT | 1999 |
|
RU2151157C1 |
Authors
Dates
1997-12-27—Published
1992-11-24—Filed