FIELD: production of granulated active aluminium oxide. SUBSTANCE: aluminium hydroxide is affected by mechanic activation, calcined at 280-550 C and is treated by peptizing agent. The process is followed by granulation and by drying. Polyvinyl alcohol is used as said peptizing agent. EFFECT: improved efficiency. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PHOSPHORIC ACID CONCENTRATION | 1992 |
|
RU2008255C1 |
METHOD OF PRODUCING GRANULAR ACTIVE ALUMINUM OXIDE | 2021 |
|
RU2766630C1 |
METHOD OF OBTAINING GRANULAR SORBENT | 2012 |
|
RU2503619C1 |
METHOD OF SULFONATED COAL PRODUCING | 1992 |
|
RU2010000C1 |
METHOD FOR CONTROL OF PRODUCING MONO- AND DIAMMONIUMPHOSPHATE SOLUTIONS | 1991 |
|
RU2006460C1 |
GRANULATED SORBENT PRODUCING METHOD | 2014 |
|
RU2578691C1 |
METHOD OF PURIFICATION OF EXHAUST GASES FROM HYDROGEN FLUORIDE AND SILICON TETRAFLUORIDE | 0 |
|
SU1820858A3 |
DEVICE FOR PRODUCTION OF AMMONIUM PHOSPHATES | 1991 |
|
RU2022919C1 |
METHOD OF SYNTHESIS OF SULFURIC ACID BY NITROSOUS METHOD | 1993 |
|
RU2042610C1 |
METHOD FOR PREPARING CATALYST FOR HYDROCARBON CONVERSION | 1990 |
|
SU1780208A1 |
Authors
Dates
1998-02-27—Published
1993-02-09—Filed