FIELD: production of protective concrete which may be used as protection against ionized irradiation. SUBSTANCE: mixture comprises, mas.%: portland cement, 37.04-39.17; schungisite dust (having specific surface 2800 cm2/g and particles being 50-250 mcm in size), 12.28-13.21; schungisite sand (size of particles being 0.14-2.5 mm), 29.45-31.68; superpeptizing additive, 0.259-0.274; saponified woody resin being used as air-implicating additive, 0.018-0.02, boron carbide having formula B4C, 1.68-1.73; water, 17.7-18.8. Compressive strength of samples being irradiated by 3500 Mrad dose in a year is up to 26.7 MPa, their tensile strength is up to 5.2 MPa, waterproofness is up to 10.0 kgf/cm2, gas permeability is up to 4.2 s/cm3. EFFECT: improved quality. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
DECORATIVE TILEBOARD AND MIXTURE USED FOR MANUFACTURE THEREOF (VERSIONS) | 2007 |
|
RU2355852C2 |
SORBING CONCRETE MIX | 1996 |
|
RU2117645C1 |
DRY BUILDING MIX (VERSIONS) | 2006 |
|
RU2307809C1 |
CONSTRUCTION MATERIAL COMPOSITION | 2014 |
|
RU2575857C2 |
CONTAINER FOR STORAGE AND TRANSPORT OF SPENT FUEL ASSEMBLIES | 1998 |
|
RU2154316C2 |
COMPLEX ADDITIVE FOR CONCRETE MIXTURE | 2008 |
|
RU2390509C2 |
CONCRETE MIXTURE, ADDITIVE FOR CONCRETE MIXTURE AND CEMENT MODIFIED WITH SAME ADDITIVE (VARIANTS) | 2003 |
|
RU2247090C1 |
MORTAR | 2011 |
|
RU2478593C1 |
CONCRETE COMPOSITION (VERSIONS) | 2008 |
|
RU2365554C1 |
DRY BUILDING MIXTURE FOR MAINTENANCE AND REPAIR WORK | 2008 |
|
RU2369575C1 |
Authors
Dates
1998-03-20—Published
1995-07-19—Filed