FIELD: protection of articles from abrasive wear and high-temperature corrosion; applicable in aviation, mechanical engineering, automotive and other industries. SUBSTANCE: the offered method is realized by microarc oxidation with voltage of coating formation of 160-170 V and current density of 0.9-1.2 A/sq.cm in electrolyte based on sodium hexafluoroaluminate with electrolyte pH 9.8-10.2. Electrolyte contains the following components, g/l: sodium hexafluoroaluminate 2.0-12.0; potassium tartrate 5.0-10.0; sodium fluoride 0.5-2.0; potassium hydroxide 0.5-0.6. Formation in composition of coating of glass phase based on aluminum oxide modified with fluorine allows production of protective anticorrosive coatings possessing high microhardness and heat resistance. EFFECT: higher efficiency. 2 tbl
| Title | Year | Author | Number | 
|---|---|---|---|
| ELECTROLYTE FOR DEPOSITION OF COATINGS ONTO VALVE METALS | 1992 | 
 | RU2046156C1 | 
| METHOD FOR OBTAINING PROTECTIVE COATING ON VALVE METALS AND THEIR ALLOYS | 1992 | 
 | RU2049162C1 | 
| METHOD OF APPLYING OPTICALLY BLACK PROTECTIVE COATINGS ONTO VALVE METALS | 1996 | 
 | RU2096534C1 | 
| METHOD OF MAKING PROTECTIVE COATINGS ON VALVE METALS AND ALLOYS THEREOF | 2017 | 
 | RU2677388C1 | 
| PROCESS OF MANUFACTURE OF TINTED COAST ON VALVE METALS AND ALLOYS | 1993 | 
 | RU2066716C1 | 
| METHOD OF APPLICATION OF PROTECTIVE COATINGS BASED ON ALUMINUM AND ITS ALLOYS | 2004 | 
 | RU2263164C1 | 
| PROCESS OF MICROARC MANUFACTURE OF PROTECTIVE FILMS ON SURFACES OF METALS AND THEIR ALLOYS | 1991 | 
 | RU2061107C1 | 
| METHOD OF RECEIVING OF PROTECTIVE COATING ON MAGNESIUM ALLOYS | 2008 | 
 | RU2357016C1 | 
| ELECTROLYTE FOR MICROARC OXIDATION OF TITANIUM AND ITS ALLOYS | 1988 | 
 | SU1788793A1 | 
| METHOD FOR OBTAINING PROTECTIVE POLYMER-CONTAINING COATINGS ON METALS AND ALLOYS | 2014 | 
 | RU2569259C1 | 