FIELD: construction ceramics. SUBSTANCE: method is designed to provide material for manufacturing wear and chemically resistant parts of equipment to stand high static loads. When preparing corundum ceramics batch with reduced sintering temperature (1500-1550 C), silica (92-96 wt %) is used which is mixed with glass additive-mineralizer (3-6%) preliminarily sintered at 900-1000 C and fluoride-containing additive (0.5-1%). Glass additive contains calcium, silicon, and boron oxides at 1:1:1 ratio. EFFECT: reduced sintering temperature with no loss in strength characteristics. 1 tbl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING CORUNDUM CERAMIC MATERIAL | 2000 |
|
RU2171244C1 |
BLEND FOR PREPARING STRUCTURAL ALUMINA CERAMIC MATERIAL AND METHOD OF MANUFACTURING PRODUCTS MADE THEREOF | 2000 |
|
RU2168483C1 |
BAUXITE CONCENTRATION PROCESS | 1997 |
|
RU2136378C1 |
METHOD OF CORUNDUM CERAMICS PRODUCING | 1996 |
|
RU2100315C1 |
METHOD FOR PRODUCING STRUCTURAL CERAMICS BASED ON ALUMINUM OXIDE | 2022 |
|
RU2789475C1 |
METHOD OF PRODUCING ALUMINA CERAMIC | 2012 |
|
RU2494994C1 |
CHARGE BASED ON ALUMINUM OXIDE AND METHOD FOR ITS PRODUCTION | 2021 |
|
RU2775746C1 |
MIXTURE FOR PRODUCTION OF SHOCK-VISCOUS CORUNDUM CERAMICS | 1995 |
|
RU2096383C1 |
METHOD OF PRODUCTION OF ARTICLES ON BASE OF ALUMINUM OXIDE | 2006 |
|
RU2322422C2 |
METHOD OF PRODUCING ALUMINA CERAMIC | 2009 |
|
RU2405756C1 |
Authors
Dates
1998-10-10—Published
1997-06-10—Filed