FIELD: ferrous metallurgy. SUBSTANCE: hearth is washed with washing agglomerate sintered from charge containing, wt %: fire scale, 82-84; iron-ore concentrate, 7.6-8.2; manganese ore, 4.3-4.6; crude fluxes (limestone-dolomite mixture), ≤ 4.0. Washing agglomerate is loaded into furnace by substituting ore components in 3 to 20 charges daily while ore to coke ratio is reduced by 5-10%. Duration of washing ranges from 3 to 15 days in dependence on hearth condition. EFFECT: increased productivity, reduced specific coke consumption, and improved quality of cast iron. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF FLUSHING OF BLAST-FURNACE HEARTH | 1998 |
|
RU2136761C1 |
METHOD OF WASH OF BLAST-FURNACE HEARTH | 1996 |
|
RU2112044C1 |
METHOD OF WASHING THE BLAST FURNACE HEARTH | 2005 |
|
RU2303070C2 |
METHOD OF WASHING BLAST FURNACE HEARTH AND WALLS | 0 |
|
SU1186635A1 |
METHOD TO PRODUCE WUSTITE PRODUCT FOR FLUSHING OF BLAST FURNACE HEARTH | 2012 |
|
RU2516428C2 |
BLAST-FURNACE MELTING METHOD OF TITANIUM-BEARING IRON-ORE RAW MATERIALS | 2007 |
|
RU2351657C2 |
BLAST-FURNACE SMELTING METHOD | 2013 |
|
RU2544972C2 |
METHOD OF BLUST-FURNACE HEARTH FLUSHING | 2007 |
|
RU2343199C1 |
METHOD FOR WASHING OF HEARTH OF BLAST FURNACE | 1992 |
|
RU2071973C1 |
METHOD OF WASHING HEARTH OF BLAST FURNACE | 0 |
|
SU802365A1 |
Authors
Dates
1998-10-10—Published
1997-07-29—Filed