FIELD: heat treatment of structures made of age-hardenable alloys and operating under conditions of high and low temperatures, vibration and corrosive media, particular, treatment of soldered-welded structures having parts of maraging steel and age-hardenable nickel alloy. SUBSTANCE: the claimed method includes heating of structure for soldering or welding up to temperature of 1200 ± 10 C, holding at this temperature for 6-9 min, and cooling at cooling rate of 50-70 C/min. Further on, structure is subjected to double heating up to temperature of 860 ± 10 C, holding at this temperature for 4-5 h and cooling in the air. Then, it is treated with cold at temperature of minus 50 minus 70 C for 2-3 h and tempering at temperature of 200-250 C for 2-3 h. EFFECT: high enough mechanical characteristics of soldered-welded structure serviceable under extreme operating conditions without failure. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR SOLDERING REFRACTORY DISPERSION-HARDENED NICKEL-CHROME BASE ALLOYS | 1996 |
|
RU2129061C1 |
METHOD FOR MAKING SOLDERED AND WELDED CONSTRUCTION | 2000 |
|
RU2184021C2 |
PROCESS FOR MANUFACTURING CORRUGATED PIPES | 1993 |
|
RU2063284C1 |
PART SOLDERING METHOD | 1993 |
|
RU2051013C1 |
METHOD OF SOLDERING OF TELESCOPIC STRUCTURES | 1996 |
|
RU2094190C1 |
SOLDER FOR PARTS SOLDERING | 1996 |
|
RU2129482C1 |
METHOD OF MAKING SOLDERED TELESCOPIC STRUCTURES | 1996 |
|
RU2109606C1 |
PROCESS OF SOLDERING OF TELESCOPIC STRUCTURES | 1996 |
|
RU2106941C1 |
METHOD FOR MANUFACTURE OF SOLDERED TELESCOPIC CONSTRUCTION | 1996 |
|
RU2106230C1 |
SOLDER FOR SOLDERING OF COPPER-STEEL ARTICLES | 1996 |
|
RU2129063C1 |
Authors
Dates
1999-04-20—Published
1997-04-02—Filed