FIELD: metallurgical industry. SUBSTANCE: nickel-based alloy comprises (wt %): nickel base, tungsten, 11.8-12.4; cobalt, 9.7-10.3; aluminium 4.9-5.2; chromium 8.7-9.6; tantalum, 0.9-1.1; molybdenum, 1.4-1.6; titanium, 2.16-2.36; niobium, 1.1- 1.4; vanadium, 0.2-0.24; hafnium, 0.03-0.06; zirconium, 0.12-0.15; cerium, 0.01-0.02; boron, 0.02-0.04; carbon, 0.18-0.26; titanium carbide, 1.00-1.10; tantalum carbide, 0.5-0.6. EFFECT: longer service life of stamping equipment during isothermal deformation and greater strength, higher heat resistance and higher wear resistance of the alloy. 8 tbl
| Title | Year | Author | Number | 
|---|---|---|---|
| NICKEL-BASED REFRACTORY ALLOY | 1995 | 
 | RU2088685C1 | 
| COMPOSITION OF HEAT-RESISTANT NICKEL ALLOY (VERSIONS) | 2007 | 
 | RU2353691C2 | 
| COMPOSITION OF CAST HEAT RESISTANT ALLOY ON NICKEL BASE | 2006 | 
 | RU2344190C2 | 
| METHOD OF TREATMENT OF CASTS OUT OF HEAT RESISTANT ALLOY | 2007 | 
 | RU2344195C2 | 
| METHOD OF PRODUCING NICKEL HEAT RESISTANT ALLOY | 2007 | 
 | RU2344188C2 | 
| DEFORMABLE NICKEL-BASED HEAT-RESISTANT ALLOY | 2019 | 
 | RU2695097C1 | 
| HEAT-RESISTANT NICKEL-BASE WROUGHT ALLOY AND ARTICLE MADE FROM THIS ALLOY | 2008 | 
 | RU2365657C1 | 
| CONTENT OF HEAT-RESISTANT NICKEL ALLOY FOR SINGLE-CRYSTAL CASTING (VERSIONS) | 2007 | 
 | RU2348725C2 | 
| HEAT RESISTANT NICKEL-BASED ALLOY FOR PRODUCING BOILER PARTS AND STEAM TURBINES OPERATING UNDER ULTRA-SUPERCRITICAL STEAM PARAMETERS | 2017 | 
 | RU2637844C1 | 
| INTERMETALLIC ALLOY BASED ON NICKEL-ALUMINIUM-COBALT SYSTEM | 2015 | 
 | RU2603415C1 | 
Authors
Dates
1999-05-10—Published
1997-10-23—Filed