FIELD: mechanical engineering; production of welded titanium constructions. SUBSTANCE: welding of titanium alloys is carried out with nonconsuming flat-tyre electrode with two tips arranged in tandem is argon atmosphere. Distance between electrode tips is found from equation t ≤ 0,013•Iw where t is tip-to-tip distance, mm; Iw is welding current, A; 0.013 is argon-arc welding coefficient, mm/a. EFFECT: elimination of hydrogen porosity, possibility of dispensing with operations for preparing surfaces to be butt-welded, and correction of welding defects. 1 cl, 1 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF ONE-PASS ARC WELDING OF TITANIUM AND TITANIUM ALLOY ARTICLES OF THICKNESS FROM 10 MM AND GREATER OVER GAS-SATURATED EDGES | 1999 |
|
RU2156680C1 |
EXTENSION STRIP FOR WELDING BY MEANS OF NON-CONSUMABLE ELECTRODE | 1998 |
|
RU2153408C2 |
METHOD OF FUSION WELDING OF METALS AND ALLOYS UNDERGONE POLYMORPHIC TRANSFORMATION | 1996 |
|
RU2110379C1 |
DIPPED ELECTRODE WELDING METHOD | 1994 |
|
RU2113951C1 |
TUNGSTEN ELECTRODE | 1999 |
|
RU2162779C2 |
NONCONSUMABLE ELECTRODE FOR WELDING IN INERT GASES | 2001 |
|
RU2193479C1 |
METHOD FOR PREPARING FOR WELDING EDGES OF SHEET BLANKS OF TITANIUM ALLOYS | 2001 |
|
RU2196032C1 |
METHOD OF TITANIUM ALLOYS BLANKS PREPARATION FOR WELDING | 1992 |
|
RU2076029C1 |
ARGON ARC WELDING METHOD | 2001 |
|
RU2201320C1 |
METHOD OF DIFFUSION WELDING OF METALS AND ALLOYS | 1996 |
|
RU2135337C1 |
Authors
Dates
1999-07-20—Published
1997-12-09—Filed