FIELD: titanium alloys welding. SUBSTANCE: blanks for welding are subjected to heating in air medium under temperature 150 - 300 C and 1 - 3 hour holding correspondingly. As a version heating is exercised immediately after blanks shearing after scraping, clarification or after hydraulic sand-blasting or shot-blasting clearing. EFFECT: improved process. 3 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PREPARING FOR WELDING EDGES OF SHEET BLANKS OF TITANIUM ALLOYS | 2001 |
|
RU2196032C1 |
METHOD OF APPLICATION OF PROTECTIVE COATS ON SURFACES OF BLANKS MADE FROM TITANIUM AND ITS ALLOYS | 1999 |
|
RU2176285C2 |
METHOD OF ONE-PASS ARC WELDING OF TITANIUM AND TITANIUM ALLOY ARTICLES OF THICKNESS FROM 10 MM AND GREATER OVER GAS-SATURATED EDGES | 1999 |
|
RU2156680C1 |
TITANIUM ALLOY ARGON ARC WELDING METHOD | 1997 |
|
RU2133178C1 |
METHOD FOR DRAWING PARTS OF SHEET BLANKS | 1998 |
|
RU2148460C1 |
METHOD FOR FLANGING OPENINGS IN SHEET BLANK | 1998 |
|
RU2153405C2 |
DIPPED ELECTRODE WELDING METHOD | 1994 |
|
RU2113951C1 |
METHOD OF FUSION WELDING OF METALS AND ALLOYS UNDERGONE POLYMORPHIC TRANSFORMATION | 1996 |
|
RU2110379C1 |
BLANK FOR SHEET FORMING WITH USE OF RESISTANCE HEATING | 1993 |
|
RU2090286C1 |
TITANIUM ALLOY PIPE EXPANDING DIE | 1996 |
|
RU2104815C1 |
Authors
Dates
1997-03-27—Published
1992-04-14—Filed