FIELD: metallurgy. SUBSTANCE: method involves hot rolling; intensified cooling; winding strip into roll; cooling roll; unwinding roll and cutting it into measured lengths; normalizing in two stages: first stage at A(C3) + 30-50 C, second stage at temperature ranging between critical points of A(C1) and A(C3). Method allows metal with completely spheroidized pearlite structure to be produced. EFFECT: increased efficiency of thermal treatment process and reduced power consumption. 1 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF TREATING ROLLED PRODUCTS FOR FINISH STAMPING | 0 |
|
SU1178781A1 |
PROCEDURE FOR PRODUCTION OF LOW CARBON COLD ROLLED STEEL FOR PRESS FORMING AND SUCCESSIVE ENAMELLING | 2010 |
|
RU2424328C1 |
METHOD OF PRODUCING A PIPE WITH LOW YIELD POINT TO ULTIMATE STRENGTH RATIO | 2018 |
|
RU2682984C1 |
MANUFACTURING METHOD OF HOT-ROLLED PIPE STEEL | 2011 |
|
RU2440425C1 |
METHOD OF PRODUCTION OF COLD-ROLLED ELECTRICAL-SHEET NON-ORIENTED STEEL | 2002 |
|
RU2219253C2 |
METHOD OF MAKING ISOTROPIC ELECTRICAL STEEL | 2001 |
|
RU2203332C2 |
METHOD OF PRODUCTION OF COLD-ROLLED ELECTRICAL ISOTROPIC STEEL | 2002 |
|
RU2228374C2 |
STRIP HOT ROLLING PROCESS | 2004 |
|
RU2267368C1 |
METHOD OF MANUFACTURE OF WIDE-STRIP LOW-CARBON STEEL | 1999 |
|
RU2144090C1 |
MANUFACTURING METHOD OF COLD-ROLLED STRIP FOR COLD BLANKING | 2012 |
|
RU2479643C1 |
Authors
Dates
1999-07-20—Published
1998-01-20—Filed