FIELD: nuclear power engineering. SUBSTANCE: method involves crushing operations, removal of defective graphite blocks, and installation of substituting ones. Substituting blocks are conveyed to installation site by their horizontal displacement in adjacent units under top biologic shield of reactor starting from passage in upper metal structure of reactor up to defective unit with process channels removed. Upon ceasing displacement, stack of graphite blocks under passage is filled with missing graphite blocks. In this way, entire graphite stacking or most of its blocks can be replaced by new ones in pressure-tube reactors. EFFECT: improved labor productivity and facilitated procedure. 10 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR RETROFITTING URANIUM-GRAPHITE REACTOR CORE | 1998 |
|
RU2147147C1 |
MECHANICAL DESIGN OF GRAPHITE-URANIUM REACTOR CORE | 1998 |
|
RU2161831C2 |
METHOD FOR RECOVERING SERVICEABILITY OF EXPANSION DEVICE IN PROCESS CHANNEL OF URANIUM-GRAPHITE REACTOR | 1996 |
|
RU2105358C1 |
PROCESS OF REPAIR OF GRAPHITE STACKING OF ACTIVE ZONE OF CHANNEL NUCLEAR REACTOR | 1993 |
|
RU2035071C1 |
REPAIR METHOD FOR GRAPHITE STACKING OF NUCLEAR URANIUM-GRAPHITE REACTOR CORE | 1991 |
|
RU2029997C1 |
SUPPORTING INSERT FOR RECOVERING VERTICAL COMPENSATING CAPACITY OF NUCLEAR REACTOR GRAPHITE STACKING AND TOOL FOR ITS INSTALLATION | 1996 |
|
RU2117340C1 |
REPAIR METHOD FOR GRAPHITE BLOCKS OF PRESSURIZED-TUBE NUCLEAR REACTOR | 1993 |
|
RU2083003C1 |
VERTICAL SAFETY CHAMBER | 2000 |
|
RU2186432C2 |
GEAR FOR CRUSHING OF DEFECTIVE GRAPHITE BLOCKS OF STACKING OF NUCLEAR URANIUM-GRAPHITE REACTOR | 1991 |
|
RU2027234C1 |
METHOD EVALUATING RESISTANCE OF STEELS AND ALLOYS TO INTERCRYSTALLINE CORROSION CRACKING | 1998 |
|
RU2137110C1 |
Authors
Dates
1999-09-10—Published
1998-06-15—Filed