FIELD: manufacture of building materials. SUBSTANCE: mix contains carbonate, iron-containing and alumino-silicate components, the latter being in the form of blast-furnace slag (50.0-85.0%) and gold-slag rejects (15.0-50.0) not undergoing phase conversions within temperature range up to 1200 C. EFFECT: intensified clinker formation process due to appearance of low-basicity liquid phase. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCTION OF PORTLAND CEMENT CLINKER | 1996 |
|
RU2114078C1 |
PORTLAND CEMENT CLINKER PRODUCTION PROCESS | 2001 |
|
RU2198146C2 |
METHOD OF PREPARING PORTLAND CEMENT CLINKER | 1998 |
|
RU2151113C1 |
RAW MILL FOR MANUFACTURING PORTLAND CEMENT CLINKER | 2002 |
|
RU2207994C1 |
FEEDSTOCK MIXTURE FOR PRODUCING CEMENT CLINKER | 1997 |
|
RU2101247C1 |
RAW MIX FOR PREPARING PORTLAND CEMENT CLINKER | 0 |
|
SU1031933A1 |
RAW MIX FOR OBTAINING PORTLAND CLINKER | 0 |
|
SU639829A1 |
RAW MIXTURE FOR PRODUCING PORTLANDCEMENT CLINKER | 0 |
|
SU796205A1 |
METHOD FOR PRODUCTION OF CEMENT AND RAW MEAL FOR MANUFACTURING CEMENT CLINKER | 1998 |
|
RU2138457C1 |
RAW MIXTURE FOR PRODUCING PORTLANDCEMENT CLINKER | 0 |
|
SU783262A1 |
Authors
Dates
1999-09-20—Published
1998-04-08—Filed