FIELD: production of portland cement clinker. SUBSTANCE: method includes supply to furnace of raw material mixture in two flows. In so doing, raw material mixture supplied from the furnace cold end has saturation coefficient of 0.92-2.10, and raw material mixture supplied to hot zone with temperature of 550-1200 C is presented in the form of low-melting charge which consists of fuel-containing products and technogenic materials with saturation coefficient of 0.05-0.5 and melting temperature of 1100-1150 C in points of high-temperature contact of charge ingredients or products of their heat treatment. EFFECT: intensified formation of clinker.
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING PORTLAND CEMENT CLINKER | 1998 |
|
RU2151113C1 |
RAW MIX FOR MANUFACTURING DRY-METHOD PORTLAND CEMENT CLINKER | 1998 |
|
RU2137728C1 |
PORTLAND CEMENT CLINKER PRODUCTION PROCESS | 2001 |
|
RU2198146C2 |
METHOD FOR PREPARING PORTLAND CEMENT CLINKER | 2001 |
|
RU2215704C2 |
METHOD FOR PRODUCING PORTLAND CEMENT CLINKER | 2022 |
|
RU2783930C1 |
METHOD FOR PRODUCING PORTLAND CEMENT CLINKER | 2022 |
|
RU2783929C1 |
METHOD OF PRODUCING PORTLAND CEMENT | 2020 |
|
RU2742384C1 |
0 |
|
SU513950A1 | |
SULFOALUMINATE CLINKER ON THE BASIS OF INDUSTRIAL WASTES OBTAINED BY MEANS OF DISSOLVING | 2010 |
|
RU2442759C2 |
METHOD OF PRODUCING PORTLANDCEMENT CLINKER | 0 |
|
SU833681A1 |
Authors
Dates
1998-06-27—Published
1996-12-04—Filed