FIELD: protective coatings. SUBSTANCE: composition for erosion-resistant coatings for porous oxide materials includes 75-85% of apatite flotation slime and 15-25% of manganese borate additive, the former being composed of, wt %: silicon oxide 40.6-41.7, aluminum oxide 22.1-23.0, iron oxide 5.5-6.0, titanium dioxide 3.6-4.0, calcium oxide 4.7-5.3, sodium oxide 12.6-13.8, potassium oxide 5.6-6.3, and phosphorus pentoxide 2.4-2.8. Coating is formed at 900 C for 15 min and preserves its properties at 900 C for more than 150 hr. EFFECT: reduced cost. 3 tbl
Title | Year | Author | Number |
---|---|---|---|
SMELT FOR BORONIZING OF ARTICLES MADE OF TITANIUM AND ITS ALLOYS | 1991 |
|
RU2031972C1 |
COATING COMPOSITION | 0 |
|
SU1331846A1 |
METHOD OF CRYSTALLINE SILICAALUMINOPHOSPHATE PREPARING | 1991 |
|
RU2024430C1 |
METHOD FOR MANUFACTURE OF GLASS-CERAMIC COMPOSITE | 2001 |
|
RU2204532C2 |
COMPOSITION FOR APPLYING PROTECTING COATING ON CARBON PRODUCTS | 1992 |
|
RU2069208C1 |
COMPOUND FOR PRODUCING EROSION RESISTANT COAT | 0 |
|
SU1759816A1 |
COATING COMPOSITE MATERIAL | 0 |
|
SU1588789A1 |
CHARGE COMPOSITION FOR PRODUCING HEAT-INSULATING BLOCKS FROM APATITO-NEPHELINE ORES PROCESSING WASTE | 2022 |
|
RU2799217C1 |
METHOD FOR PRODUCTION OF GRANULAR BUILDING MATERIAL FROM WASTE OF PROCESSING OF APATITE-NEPHELINE ORES | 2021 |
|
RU2781680C1 |
METHOD OF PRODUCTION OF GLASS-CERAMIC COATINGS | 2003 |
|
RU2260569C1 |
Authors
Dates
1999-09-27—Published
1998-05-26—Filed