FIELD: polymer production. SUBSTANCE: process involves interaction of equimolar amounts of p-phenylenediamine and terephthaloyl dichloride in solution of N-methyl-2-pyrrolidone with calcium chloride carried out in cylindrical reactor provided with single stirring motor used both as stirrer and as granulator. Stirring is effected under vortex conditions accompanied with adding terephthaloyl dichloride and disintegrating polymer product in the same reactor. Product has relative viscosity above 3.5 and is suited to manufacture high-strength long staple. EFFECT: improved consumer's property of polymer. 9 cl, 3 tbl, 5 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING POLY-P-PHENYLENETEREPHTHALAMIDE | 0 |
|
SU822756A3 |
NONFIBROUS POLYMER SOLUTION PARA-ARAMIDE WITH HIGH RELATIVE VISCOSITY | 2004 |
|
RU2342474C2 |
METHOD FOR SPINNING OF FIBRES OF FILAMENTS (MODIFICATIONS), FIBRES AND FILAMENTS (MODIFICATIONS), PULP | 1996 |
|
RU2144099C1 |
METHOD OF PREPARING INITIATOR COMPOSITIONS CONTAINING POLYVINYL ALCOHOL AND SURFACTANT | 1997 |
|
RU2205840C2 |
METHOD FOR POLYMERIZATION OF ETHYLENE-UNSATURATED MONOMERS IN PRESENCE OF DIACYLPEROXIDES AS SOURCE OF FREE RADICALS | 2003 |
|
RU2318002C2 |
PEROXIDE DOSING IN SUSPENSION METHOD ACCORDING TO WHICH STEROL IS POLYMERISED | 2004 |
|
RU2360929C2 |
METHOD OF MANUFACTURING FIBERS FROM POLY(P-PHENYLENETEREPHTHALAMIDE) | 1996 |
|
RU2161557C2 |
MIXTURE CONTAINING QUARTERNARY AMMONIUM COMPOUND AND ITS APPLICATION | 2008 |
|
RU2469990C2 |
SIZING COMPOSITION | 2000 |
|
RU2211274C2 |
FIRE RESISTANT COMPOSITE MATERIAL | 2007 |
|
RU2435801C2 |
Authors
Dates
1999-09-27—Published
1995-02-09—Filed