FIELD: chemistry industry. SUBSTANCE: plastic comprises epoxydiane resin, aromatic amine hardener and active diluent. Active diluent comprises phosphorus glycidyl acid esters of general formula: , ratio of components being as follows, wt parts: epoxydiane resin, 100; phosphorus acid glycidyl esters; aromatic amine hardener, stoichiometric amount. EFFECT: lower viscosity, shorter hardening time and higher heat resistance. 9 ex, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
INSULATION COMPOUND PREPARATION METHOD | 2003 |
|
RU2247752C1 |
HEAT-RESISTANT LOW-VISCOSITY BINDER FOR THE MANUFACTURE OF PRODUCTS BY METHODS OF VACUUM INFUSION AND IMPREGNATION UNDER PRESSURE AND A METHOD FOR ITS PRODUCTION | 2021 |
|
RU2762559C1 |
BINDING SUBSTANCE FOR REINFORCED PLASTICS | 2007 |
|
RU2338762C1 |
COMPOSITE FOR GRADIENT COVER PREPARING | 1999 |
|
RU2194731C2 |
METHOD OF PRODUCING HEAT ISOLATION GRADIENT COAT | 2009 |
|
RU2424905C1 |
METHOD FOR PRODUCTION OF POLYMERIC MATERIALS WITH REFRACTIVE INDEX GRADIENT FOR LIGHT FOCUSING ELEMENTS | 2002 |
|
RU2222430C1 |
EPOXIDE BINDER FOR GLASS PLASTICS | 2004 |
|
RU2270213C1 |
METHOD OF PRODUCING ANTI-FRICTION GRADIENT COATINGS | 2009 |
|
RU2425080C1 |
METHOD OF MAKING GRADIENT COATINGS - RUST MODIFIERS | 2011 |
|
RU2478674C2 |
OPTICAL ADHESIVE | 1998 |
|
RU2141989C1 |
Authors
Dates
1999-11-20—Published
1998-05-07—Filed