FIELD: production of composite materials. SUBSTANCE: annuals are treated with water or steam at 40 to 120 C at simultaneous or subsequent highly shearable treatment followed by heating and compression of treated residual in presence of binder. EFFECT: improved properties of annual fibers. 7 cl, 7 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF UTILIZING RECYCLING LIGNOCELLULOSE COMPOSITE MATERIALS | 1997 |
|
RU2165352C2 |
METHOD OF PRODUCING PLATE COMPOSITE MATERIAL FROM LIGNOCELLULOSES | 2008 |
|
RU2404048C2 |
METHOD OF PRODUCING IMPROVED COMPOSITE PLATES | 2017 |
|
RU2732337C2 |
COMPOSITION FOR COATING AND SEALING EDGES OF FIBERBOARDS | 2019 |
|
RU2781067C2 |
COMPOSITE ADHESIVE AND USE THEREOF IN COMPOSITE WOOD BOARDS | 2011 |
|
RU2586146C2 |
METHOD FOR BINDING LIGNOCELLULOSE MATERIALS WHEN USING POLYISOCYANATE COMPOSITIONS | 2018 |
|
RU2771367C2 |
FIRE-RETARDANT MIXTURE FOR LIGNOCELLULOSE COMPOSITES | 2004 |
|
RU2350636C2 |
METHOD FOR PRODUCING FIBROUS SEMI-FINISHED PRODUCT FROM PLANT RAW MATERIALS | 2022 |
|
RU2809473C1 |
FIBROUS PLASTICIZED GYPSUM COMPOSITION | 2011 |
|
RU2600947C2 |
METHOD OF ADJUSTING TACK VALUE OF BINDER COMPOSITION | 2012 |
|
RU2621691C2 |
Authors
Dates
1999-12-20—Published
1997-04-10—Filed