FIELD: chemical power supplies. SUBSTANCE: method for eliminating voltage dip during initial stage of discharge of Li- CuO chemical current supply at low temperatures is implemented by treatment of finished but not yet sintered oxide-copper plate in sulfur vapors at 295 ± 15 C for 1-10 min followed by removal of sulfur portion that has not entered in reaction and final sintering of plate in open air at 295 ± 15 C for 1-10 min. EFFECT: provision for eliminating voltage dip. 1 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD FOR REDUCING OPEN-CIRCUIT VOLTAGE OF CHEMICAL CURRENT SUPPLY | 1998 |
|
RU2151452C1 |
| METHOD FOR MANUFACTURING POSITIVE PLATE OF Li/SO BATTERY | 2003 |
|
RU2249885C2 |
| METHOD FOR PRODUCING POSITIVE PLATE OF Li/SOCl SYSTEM CELL | 2004 |
|
RU2265919C1 |
| LITHIUM CURRENT SOURCE TESTING METHOD | 2013 |
|
RU2551702C2 |
| PROCESS OF PREPARATION OF ELECTROLYTE SOLUTION FOR Li/SO CHEMICAL SOURCE OF ELECTRIC ENERGY | 1999 |
|
RU2161845C1 |
| METHOD FOR MANUFACTURING Li/LiIAlCl nSO/Cu, C SYSTEM BATTERY | 2003 |
|
RU2259618C2 |
| POSITIVE ELECTRODE OF CHEMICAL SOURCE OF ELECTRIC ENERGY | 1994 |
|
RU2099819C1 |
| METHOD FOR PREPARING ELECTROLYTE FOR Li/SO STORAGE BATTERY | 2003 |
|
RU2248071C2 |
| LITHIUM CELL | 2002 |
|
RU2218634C2 |
| CHEMICAL CURRENT SOURCE | 1994 |
|
RU2057381C1 |
Authors
Dates
2000-06-20—Published
1998-04-14—Filed